LOI A ME KA LAAELA | EN ISO 10545-2 | ±0.6% | -0.1% ~+0.05% |
±2mm | 0.55 | ||
KA MANAWALEA | EN ISO 10545-2 | ±5% | -4.2% ~-3.1% |
±0.5mm | -0.4mm | ||
POLOLEI O NA aoao | EN ISO 10545-2 | ±0.5% | -0.02% ~+0.04% |
±1.5mm | 0.22mm | ||
NA WAIWAI KINO | |||
KA WAI | EN ISO 10545-3 | 0.5% | 0.5% |
IKAIKA HAHA | EN ISO 10545-4 | ≥1,100 | 1538 |
NA MAKEMAKE O KA HAEHAE | EN ISO 10545-4 | ≥30N/mm² | 36 |
KUE I KA ABRASION | EN lSO 10545-7 | HOIKE I KA PAPA ABRASION | Papa 3 |
UA HALA NA PALAPALA HOIKE | 1,500r | ||
KU'E ANA I KA HA'EHA | EN ISO 10545-9 | ʻAʻole pono e ʻike ʻia kahi kīnā | HALA |
KU'I HUI | EN ISO 10545-12 | ʻAʻohe Kēkē o ka ili a i ʻole E ʻike ʻia nā māwae | HALA |
SLIDER 96 SLIP RESISTANCE,HOAO PENDULUM PULU | E like me ka AS 4586:2013 | - | |
MATA | P2 | ||
NA WAIWAI KEMIIKA | |||
KUE KEMIIKA I NA KIMIKA HALE & PAAKAI AUAU | EN ISO 10545-13 | MINIMUM GB | A |
KUE I KA HUI | EN ISO 10545-14 | PAPA MINIMA 3 | PAPA 4 |
KAHIKI | NUI | PCS/CTN | M²/ CTN | M²/ PLT | CTN /PLT | KG/PLT |
VANCOUVER | 600x600mm/24"x24" | 4 | 1.44 | 57.6 | 40 | 1260 |
300x600mm/12"x24" | 8 | 1.44 | 57.6 | 40 | 1260 | |
300x300mm/12"×12" NO KA MAKEMAKE | 12 | 1.08 | 60.48 | 56 | 1288 | |
300×300mm/12"×12”MOSAIC | 11 | 1 | 54 | 54 | 1053 |
* Hiki ke ʻokoʻa ka nui, ke kaumaha, ka waihoʻoluʻu, ke ʻano, ka veining, ka ʻano, ka lōʻihi, ka nui, ka ʻili a me ka hoʻopau ʻana mai ka pūʻulu a i ka pūʻulu.He hōʻailona nā helu paheʻe a ʻokoʻa paha no kēlā me kēia pūʻulu tile.Manaʻo ʻia e hana ʻia kahi hoʻāʻo hou no kēlā me kēia pūʻulu tile inā koi ʻia kahi palapala hōʻike slip rating.ʻO nā kiʻi huahana i hōʻike ʻia no nā kumu hoʻohālike wale nō a ʻaʻole ia he hōʻike pololei o ka huahana.