CHARAKTERYSTYKA TECHNICZNA | METODA BADANIA | STANDARD | NEX-GEN |
WYMIARY I WYGLĄD POWIERZCHNI | |||
DŁUGOŚĆ I SZEROKOŚĆ | EN ISO 10545-2 | ±0,6% | +0,02% ~+0,03% |
±2 mm | +0,2 mm | ||
GRUBOŚĆ | EN ISO 10545-2 | ±5% | -2,7% ~+0,2% |
±0,5 mm | -0,3 mm | ||
PROSTOTNOŚĆ BOKÓW | EN ISO 10545-2 | ±0,5% | -0,05% ~+0,02% |
±1,5 mm | -0,28 mm ~ + 0,13 mm | ||
WŁAŚCIWOŚCI FIZYCZNE | |||
ABSORPCJA WODY | EN ISO 10545-3 | ≤0,5% | ≤0,1% |
WYTRZYMAŁOŚĆ | EN ISO 10545-4 | ≥1300N | 1950 |
MODUŁ PĘKNIĘCIA | EN ISO 10545-4 | ≥35 N/mm² | 48 |
ODPORNOŚĆ NA ŚCIERANIE | EN ISO 10545-7 | ZGŁOŚ DO KLASY ŚCIERALNOŚCI | klasa 4 |
PRZEKONANE CYKLE RAPORTÓW | 2100r | ||
ODPORNOŚĆ NA SZOK TERMICZNY | EN ISO 10545-9 | ŻADNA WADA NIE POWINNA BYĆ WIDOCZNA | PRZECHODZIĆ |
ODPORNOŚĆ NA MROŻ | EN ISO 10545-12 | ŻADNYCH WAD POWIERZCHNIOWYCH LUB PĘKNIĘCIA POWINNY BYĆ WIDOCZNE | PRZECHODZIĆ |
SUWAK 96 ANTYPOŚLIZGOWY, BADANIE WAHADŁEM MOKRYM | ZGODNIE Z AS 4586:2013 | - | |
MAT | P2 | ||
ZEWNĘTRZNY | P4 | ||
WŁAŚCIWOŚCI CHEMICZNE | |||
ODPORNOŚĆ CHEMICZNA DO CHEMII GOSPODARSTWA I SOLE DO BASENÓW | EN ISO 10545-13 | MINIMUM GB | A |
ODPORNOŚĆ NA PLAMOWANIE | EN ISO 10545-14 | KLASA MINIMALNA 3 | KLASA 4 |
SERIA | ROZMIARY | SZT/CTN | M²/ CTN | M²/PLT | CTN /PLT | KG/PLT | |
ZAMEK Z PIASKU | 450x450mm/18" x 18" | 7 | 1.4175 | 45.36 | 32 | 896 | |
300x300mm/12"x12" | 13 | 1.17 | 65,52 | 56 | 1232 |
*Płytki mogą różnić się rozmiarem, wagą, kolorem, wzorem, żyłkowaniem, fakturą, trwałością, gęstością, powierzchnią i wykończeniem w zależności od partii.Wskaźniki poślizgu służą jako wskazówka i mogą się różnić dla każdej partii płytek.Zaleca się przeprowadzenie nowego testu dla każdej partii płytek, jeśli wymagany jest certyfikat antypoślizgowości.Przedstawione zdjęcia produktów służą wyłącznie celom ilustracyjnym i nie stanowią dokładnego odzwierciedlenia produktu.