KARAKTERISTIKAT TEKNIKE | METODA E TESTIMIT | STANDARD | NEX-GEN |
MATJA DHE PARAQITJA E SIPËRFAQËSISË | |||
GJATESIA DHE GJERESIA | EN ISO 10545-2 | ±0,6% | -0,03% ~+0,02% |
±2 mm | -0.2mm ~+0.1mm | ||
TRASHËSIA | EN ISO 10545-2 | ±5% | -3.1% ~0 |
±0,5 mm | -0.3mm ~0 | ||
DREJTËSIA E ANËVE | EN ISO 10545-2 | ±0,5% | -0,05% ~+0,02% |
±1,5 mm | -0.28mm ~+0.13mm | ||
VETITË FIZIKE | |||
THYRTIMI I UJIT | EN ISO 10545-3 | ≤0,5% | ≤0,1% |
THYERJA E FORCËS | EN ISO 10545-4 | ≥1300N | 1940 |
MODULI I RUPTURËS | EN ISO 10545-4 | ≥35N/mm² | 37 |
REZISTENCA NDAJ gërryerjes | EN lSO 10545-7 | RAPORTI NË KLASËN E ABRAZIONIT | Klasa 4 |
CIKLET E RAPORTIT TË KALUARA | 2100 r | ||
REZISTENCA TERMIKE SHOKU | EN ISO 10545-9 | NUK DUHET TË DUHET ASNJË defekt | KALOJE |
REZISTENCA NGA NGRITJA | EN ISO 10545-12 | JO DEFEKTE SIPËRFAQËSORE OSE DUHET TË DUHEN TË PARAQITUR | KALOJE |
Rrëshqitësi 96 REZISTENCA NË RRËSHQITJE,TESTI I lavjerrësit të lagësht | SIPAS AS 4586:2013 | - | |
MATT | P3 | ||
VETITË KIMIKE | |||
REZISTENCA KIMIKE TE KIMIKAT E FAMILJEVE & KRIPËRA TË PISHINAVE | EN ISO 10545-13 | MINIMUM GB | A |
REZISTENCA NDAJ NJOLJES | EN ISO 10545-14 | KLASA MINIMUM 3 | KLASA 5 |
SERIA | PËRMASAT | PCS/CTN | M²/ CTN | M²/PLT | CTN / PLT | KG/PLT |
MIKRO CEMENT | 600x1200mm/24"x48" | 2 | 1.44 | 79.2 | 55 | 1980 |
750x1500mm/30"x60" | 2 | 2.25 | 90 | 40 | 2280 |
*Pllakat mund të ndryshojnë në madhësi, peshë, ngjyrë, model, lyerje, strukturë, qëndrueshmëri, dendësi, sipërfaqe dhe përfundim nga grupi në grup.Vlerësimet e rrëshqitjeve shërbejnë si tregues dhe mund të ndryshojnë për çdo grup pllakash.Rekomandohet që të kryhet një test i ri për çdo grup pllakash nëse kërkohet një certifikatë e vlerësimit të rrëshqitjes.Imazhet e treguara të produktit janë vetëm për qëllime ilustrimi dhe nuk janë një paraqitje e saktë e produktit.