KARAKTERISTIKAT TEKNIKE | METODA E TESTIMIT | STANDARD | NEX-GEN |
MATJA DHE PARAQITJA E SIPËRFAQËSISË | |||
GJATESIA DHE GJERESIA | EN ISO 10545-2 | ±0,6% | -0,26% ~-0,14% |
±2 mm | -0.5mm ~+0.6mm | ||
TRASHËSIA | EN ISO 10545-2 | ±5% | -0.4% ~+0.9% |
±0,5 mm | -0.6mm ~+0.5mm | ||
DREJTËSIA E ANËVE | EN ISO 10545-2 | ±0,5% | +0,01% ~+0,03% |
±1,5 mm | +0,08mm ~+0,19mm | ||
VETITË FIZIKE | |||
THYRTIMI I UJIT | EN ISO 10545-3 | E> 10% | 15,70% |
THYERJA E FORCËS | EN ISO 10545-4 | ≥600N | 1368 |
MODULI I RUPTURËS | EN ISO 10545-4 | ≥12N/mm² | 24.9 |
REZISTENCA NDAJ gërryerjes | EN lSO 10545-7 | RAPORTI NË KLASËN E ABRAZIONIT | KLASA 3 |
CIKLET E RAPORTIT TË KALUARA | 1, 500 r | ||
REZISTENCA E CRAZHUR | EN ISO 10545-11 | REZISTENCË E PLOTË | KALOJE |
REZISTENCA NGA NGRITJA | EN ISO 10545-12 | REZISTENCË E PLOTË | KALOJE |
VETITË KIMIKE | |||
REZISTENCA KIMIKE TE KIMIKAT E FAMILJEVE & KRIPËRA TË PISHINAVE | EN ISO 10545-13 | MINIMUM GB | A |
REZISTENCA NDAJ NJOLJES | EN lSO 10545-14 KUR I SUBJEHET KIMIKAVE | KLASA MINIMUM 3 | Klasa 5 |
SERIA | PËRMASAT | PCS/CTN | M²/ CTN | Kg/Ctn | CTN / PLT | KG/PLT |
LUX | 100x100mm/4"x4" | 92 | 0,92 | 14.2 | 84 | 1218 |
76x152mm/3"x6" | 72 | 0,832 | 13.5 | 90 | 1240 |
*Pllakat mund të ndryshojnë në madhësi, peshë, ngjyrë, model, lyerje, strukturë, qëndrueshmëri, dendësi, sipërfaqe dhe përfundim nga grupi në grup.Vlerësimet e rrëshqitjeve shërbejnë si tregues dhe mund të ndryshojnë për çdo grup pllakash.Rekomandohet që të kryhet një test i ri për çdo grup pllakash nëse kërkohet një certifikatë e vlerësimit të rrëshqitjes.Imazhet e treguara të produktit janë vetëm për qëllime ilustrimi dhe nuk janë një paraqitje e saktë e produktit.