CIRI Téknis | METODE UJI | STANDAR | NEX-GEN | ||
Matt | Dipoles | Matt | Dipoles | ||
PANGUKURAN & TAMPILAN BUNGA | |||||
PANJANG JEUNG LEBAR | EN ISO 10545-2 | ± 0,6% | ± 0,6% | -0,1% ~+0,05% | -0,03% ~+0,03% |
± 2 mm | ± 2 mm | 0.55 | -0.2mm ~ + 0.2mm | ||
KETEPATAN | EN ISO 10545-2 | ± 5% | ± 5% | -4,2% ~-3,1% | -1,1% ~+1,1% |
± 0,5 mm | ± 0,5 mm | -0,4 mm | -0.1mm ~+0.1mm | ||
STRAIGHTNESS SISI | EN ISO 10545-2 | ± 0,5% | ± 0,5% | -0,02% ~+0,04% | -0,03% ~+0,04% |
± 1,5 mm | ± 1,5 mm | 0,22 mm | -0.16mm ~ + 0.21mm | ||
SIFAT FISIK | |||||
nyerep cai | EN ISO 10545-3 | 0,5% | ≤0,5% | 0,5% | ≤0,1% |
NGAREGEPKEUN | EN ISO 10545-4 | ≥1.100N | ≥1300N | 1538 | 1997 |
MODULUS RUPTURE | EN ISO 10545-4 | ≥30N/mm² | ≥35N/mm² | 36 | 48 |
Résistansi kana abrasion | EN lSO 10545-7 | LAPORAN KA KELAS ABRASION | Kelas 3 | Kelas 4 | |
LAPORAN SIKLUS LULUS | 1.500r | 2.100r | |||
Résistansi shock termal | EN ISO 10545-9 | TEU KUDU KACACATAN | LULUS | LULUS | |
Résistansi ibun | EN ISO 10545-12 | NO DEFECTS permukaan ATAWA Réték kudu ditingali | LULUS | LULUS | |
SLIDER 96 SLIP RESISTANCE,UJI PENDULUM BUSUH | NURUT AS 4586:2013 | - | - | ||
MATT | P3 | - | |||
SIFAT KIMIA | |||||
Résistansi KIMIA KA BAHAN KIMIA RUMAH TANGGA & Uyah kolam renang | EN ISO 10545-13 | MINIMUM GB | MINIMUM GB | A | A |
Résistansi pikeun ngawarnaan | EN ISO 10545-14 | KELAS MINIMUM 3 | KELAS MINIMUM 3 | KELAS 4 | KELAS 5 |
SERI | SERI | PCS/CTN | M²/ CTN | M²/ PLT | CTN/PLT | KG/PLT |
ELEGANCE | 600x600mm/24"x24" | 4 | 1.44 | 57.6 | 40 | 1.220 |
* Ubin tiasa béda-béda dina ukuran, beurat, warna, pola, urat, tékstur, daya tahan, dénsitas, permukaan sareng bérés ti bets ka bets.Slip ratings ngawula ka salaku indikasi jeung bisa rupa-rupa pikeun tiap bets ubin.Dianjurkeun yén tés anyar dipigawé pikeun tiap bets ubin lamun sertipikat rating dieunakeun diperlukeun.Gambar produk anu dipidangkeun ngan ukur kanggo ilustrasi sareng sanés ngagambarkeun persis produk.